Features of Scale Defect: It occurs more frequently on the bottom surface and the head and tail of the hot rolling, and the shape of the defect is elliptical and concave.

Cause: The primary oxide scale of the slab and the second oxide scale of the hot rolling are not removed by descaling, and they are pressed into the surface of the steel coil during rolling, showing the state after pickling.

Production process: hot rolling